Contents
1. What a PLA PVA Water-Soluble Film Extrusion Line Is and Who Buys One
The line and the film it makes
A PLA PVA water-soluble film extrusion line converts a blend of polylactic acid and polyvinyl alcohol into a thin, transparent web that dissolves when it contacts water. The film is the outer pouch of a single dose laundry pod: it holds the liquid or powder detergent through storage and handling, then disappears in the wash, releasing the product without leaving a plastic residue. The line typically includes resin drying, gravimetric feeding, one or two extruders, melt filtration and metering, a flat die, a chill roll casting station, thickness measurement, slitting, rewinding and a central control panel. Some producers cast the film and ship rolls to a pod converter, while larger operations run forming, filling and sealing immediately after casting.
Three buyer groups and their real priorities
The first buyer is a detergent brand or its contract packer, which makes laundry pods and cares most about seal integrity, dissolution time and a film that does not soften on the shelf. The second is a film converter that sells water-soluble rolls to several pod makers and needs consistent gauge, quick grade changes and reliable winding. The third is an investor or a chemical group entering biodegradable packaging, drawn by the phase out of conventional single use plastics and interested in output per hour and cost per square meter. All three depend on the same discipline: a dry, homogeneous melt and a web whose thickness and dissolution behavior repeat from one roll to the next.
2. Why Water-Soluble Film for Laundry Pods
The unit dose proposition
A laundry pod is a measured dose of detergent wrapped in a film that the consumer never removes. That design removes the guesswork of dosing, reduces spills and gives the brand a distinctive product, but it transfers a great deal of responsibility to the film. The pouch must hold a concentrated, often aggressive liquid through transport and storage, survive being handled with dry hands, and then break down fully in the wash so that no film fragment remains on the clothes or in the drainage system. Water-soluble film is the only common packaging material that meets all of those conditions at once, which is why the format grew quickly once reliable film became available.
The environmental driver and its limits
Brand owners adopted water-soluble film partly because it removes a plastic pouch from the household waste stream, and the film is designed to break down in water rather than persist as a solid fragment. That benefit is real but conditional. A film that dissolves in the wash still adds its chemical oxygen demand to the wastewater, and a film that fails to dissolve completely defeats the purpose. Producers therefore work to two targets at the same time: a dissolution profile that matches a cool, short wash cycle, and a formulation whose components are acceptable in the wash water. This is a practical reason to control the formulation and the film thickness precisely rather than chase the thinnest possible gauge.
Where the film is made
Water-soluble film is produced by casting or blowing a molten blend of the resins and plasticizers, then winding it into rolls that feed a form-fill-seal machine. Cast film is common where clarity, tight gauge and high output matter, because a chill roll sets the web quickly and a flat die gives good transverse control. Blown film is used by some producers for its lower tooling cost and the strength that biaxial orientation gives a thin web. The equipment in this guide is the extrusion line that makes the film; the forming and sealing step that turns the film into a pod is described separately, because it often sits at a different company and a different stage of the supply chain.
3. PLA, PVA and the Blend: What Each Component Does
PVA provides dissolution and barrier
Polyvinyl alcohol is the component that makes the film dissolve. It is highly polar, forms a clear, flexible film, resists many oils and solvents, and softens and disperses in water at a temperature that can be tuned through the degree of hydrolysis and the plasticizer package. A cold water soluble grade dissolves in a cool wash, while a hotter grade stays intact until the water warms. PVA also gives the film good oxygen barrier, which protects sensitive detergent ingredients. Its weaknesses are strong moisture sensitivity and a narrow thermal window: it absorbs water from humid air, and at excessive melt temperature it degrades before it flows well.
PLA contributes stiffness and cost control
Polylactic acid is a rigid, bio based polyester that brings stiffness, clarity and a lower raw material cost to the blend. On its own PLA is not water soluble at wash temperature, so it is used to adjust mechanical strength, reduce stickiness and tune how fast the film breaks down, rather than as the dissolving phase. Blending PLA into PVA lowers the overall resin cost and raises the modulus, which helps the film run through high speed forming equipment. The tradeoff is that too much PLA slows dissolution and can make the film brittle, so the ratio is a formulation decision that has to be validated against both the sealing line and the wash test.
Plasticizers, compatibilizers and the processing window
Water-soluble film is not a simple two resin mixture. Plasticizers such as glycerol and sorbitol based systems soften the PVA, lower its processing temperature and control flexibility, while compatibilizers help the polar PVA and the less polar PLA form a fine, stable dispersion rather than a phase separated web. A poor dispersion shows up as gels, streaks or weak spots that fail during forming. The additives are dosed in small percentages but have an outsized effect on tensile strength, elongation, dissolution time and blocking tendency. Wanplas recommends qualifying the full formulation on the actual extruder before fixing the screw and die geometry, because the blend rheology decides the hardware.
4. Film Formats, Thickness and Dissolution Targets
Typical pod film geometry
A laundry pod film is supplied as a roll, usually in the range of 1,000 to 1,600 millimeters wide, that is cut and formed into pockets on the filling line. Film thickness normally sits between 20 and 60 micrometers, with the exact value set by the dose weight, the pocket size and the mechanical load during sealing. Cold water grades often run from 25 to 45 micrometers, hot water grades from 30 to 55, and heavier unit dose sachets or laundry bags from 35 to 70 micrometers. A thin film saves material and dissolves faster but is harder to form without pinholes, while a thicker film is stronger but may miss a short wash cycle.
Dissolution as a specification
Dissolution is not a single number. A film has an onset temperature below which it stays intact, a time to first break, and a time to complete dispersal with no visible fragments. Buyers should specify all three together with the water temperature, agitation and water hardness of the intended test, because a film that clears in soft laboratory water can leave a residue in hard water. Shelf life matters just as much: the film must keep the same dissolution profile after months in a warehouse, which depends on moisture control during and after production as much as on the formulation itself.
5. Resin Grades, Plasticizers and Material Cost
Resin and additive price bands
PVA is the most expensive component and sets the cost floor for the film, while PLA reduces the average resin cost and adds stiffness. Plasticizers and compatibilizers are used in small doses but carry a meaningful price. The table below gives planning price bands in US dollars per metric ton for the materials used in a water-soluble pod film. Actual quotes depend on the hydrolysis grade, the supplier and the purchase volume, so these figures are for budgeting rather than for contracting.
| Material | Role in the film | Price range |
|---|---|---|
| Water soluble PVA resin | Dissolving phase and oxygen barrier | 3,200 to 6,500 US dollars per ton |
| PLA resin | Stiffness, clarity and cost control | 2,200 to 3,800 US dollars per ton |
| Plasticizer package | Flexibility and processing temperature | 1,800 to 4,500 US dollars per ton |
| Compatibilizer and stabilizer | Dispersion and thermal protection | 4,000 to 9,000 US dollars per ton |
From resin price to film cost
At a 35 micrometer gauge and a blended resin price near 3,000 US dollars per ton, the polymer in one square meter of film weighs about 30 to 40 grams and costs roughly 0.09 to 0.12 US dollars. Adding plasticizer, conversion, scrap and winding brings the cash cost to roughly 0.15 to 0.24 US dollars per square meter, with a selling price commonly in the range of 0.25 to 0.45 US dollars for a qualified water-soluble grade. Those numbers are sensitive to gauge: a five micrometer reduction saves material but can push the film into pinholes and seal failures that cost far more than the saving.
6. Complete Line Equipment Price List
What a configured line includes
A water-soluble film line costs more than a general cast film line of the same width because the drying, metering and thickness control sections are more demanding. The table below gives planning price ranges in US dollars for a 1,200 to 1,600 millimeter cast film line sized for roughly 100 to 250 kilograms per hour. The figures cover the equipment only and exclude civil works, the building and the first stock of resin. They are intended to help a buyer compare quotations on the same basis.
| Line component | Function | Typical price range (US dollars) |
|---|---|---|
| Desiccant dryer with dew point logger | Dry PVA and PLA to a measured end point | 30,000 to 75,000 |
| Vacuum loader and loss in weight feeders | Meter resin and plasticizer accurately | 18,000 to 48,000 |
| Single screw extruder with barrier screw | Melt the blend at low shear | 95,000 to 220,000 |
| Continuous screen changer and melt pump | Filter gels and steady the output | 45,000 to 110,000 |
| Coat hanger flat die with lip adjustment | Spread the melt evenly across the web | 65,000 to 175,000 |
| Chill roll casting unit with air knife | Quench and set the hot web | 85,000 to 210,000 |
| Thickness gauge and automatic die control | Hold gauge and transverse profile | 70,000 to 190,000 |
| Slitting and turret winder | Cut rolls and build stable windings | 55,000 to 140,000 |
| Chiller, air system and controls | Support cooling, handling and recipes | 45,000 to 120,000 |
Where not to economize
The dryer, the melt filtration and the thickness control are the three areas where a saving usually turns into a loss. An undersized dryer will let moisture into a resin that cannot tolerate it, a coarse screen will let gels through into a 30 micrometer web, and a manual die adjustment cannot hold the gauge that a sealing line requires. By contrast, a producer making a single wide roll for a customer who slits downstream may reasonably defer an inline slitter. Wanplas recommends allocating the budget based on the failure modes of this specific film rather than copying the configuration of a polyethylene cast line.
7. Drying, Feeding and Moisture Control
Why drying comes first
Polyvinyl alcohol is hygroscopic and polylactic acid hydrolyzes in the presence of water at melt temperature, so drying is the first and most important step on this line. Resin is normally dried to a moisture content below 0.02 percent, and the drying air is measured by its dew point rather than by clock time. A desiccant dryer with a dew point logger is preferred over a simple hot air hopper because the target is tight and the consequence of missing it is a degraded, brittle web. PLA is commonly dried around 80 to 100 degrees Celsius, and PVA grades are dried within their own supplier window, since excessive heat can yellow the material or drive off the plasticizer.
Keeping moisture out after drying
Drying the resin is only half the task. The path from the dryer to the die must not let the material pick up water again, so hoppers are closed, conveying lines are dry and the system is kept under a slight dry air blanket where practical. On humid days the reabsorption rate can be fast enough to matter within a single shift. Wanplas recommends measuring moisture at the hopper outlet, not at the dryer inlet, and treating the reading as a process variable with an alarm. This single discipline prevents a large share of the gels, bubbles and brittle film that plague water-soluble film production.
8. Extrusion, Filtration and the Flat Die
A low shear melt
The extruder has to homogenize a blend whose components have different viscosities and whose thermal stability is limited. A barrier screw with a gentle compression profile is generally used to melt the pellets without excessive shear heating, and the barrel zones are held within a narrow band because a hot spot can degrade the PVA while a cold spot leaves unmelted particles. Screw speed is kept moderate and residence time is minimized, particularly on a line that stops and starts often. A general purpose screw designed for polyethylene will often over-shear this blend and turn a good formulation into a streaky film.
Filtration and metering
A continuous screen changer removes gels and hard particles before the die, and a melt gear pump steadies the flow so that the web does not pulse. These two elements are more important here than on many commodity films because a 30 micrometer web has little tolerance for a hard inclusion, and a small output ripple becomes a visible gauge band. Screen packs are changed on a pressure trend rather than on a fixed calendar, and the pressure before the pump is logged with each roll. A rising screen pressure that is ignored will eventually push a gel through the die and condemn several hundred kilograms of film.
9. Casting, Web Formation and Film Handling
Chill roll and air knife
In cast film production the hot web leaves the die and is laid onto a temperature controlled chill roll, where an air knife or vacuum box pins it flat against the surface. The roll temperature sets the cooling rate, the clarity and the flatness of the film, and it must be held evenly across the face. A roll that is too cold can trap air and produce haze, while a roll that is too warm lets the film stick or relax unevenly. For a water-soluble film the web is softer and more sensitive than polyethylene, so the air knife pressure and the nip setting are tuned gently to avoid stretching a film that has not yet fully set.
Avoiding blocking and surface damage
Plasticized PVA film has a tendency to block, meaning that adjacent layers of a wound roll stick together and resist unwinding. The casting section can reduce this by controlling the web temperature before winding and by keeping the surface free of tacky residues, but the formulation and the winding tension are equally important. A release treated surface or a light antiblock package is often used where the film will be stored for a long period. Wanplas recommends testing a roll after a controlled storage period rather than judging release only at the machine, because blocking is a time dependent failure that appears in the customer’s warehouse.
10. Thickness Control, Gauge and Profile
Why gauge decides the economics
Film thickness is the single number that connects the machine to the cost and the performance of a laundry pod. A film that is two micrometers too thick wastes resin on every square meter, while a film that is two micrometers too thin can fail during forming or dissolve before the pod reaches the wash. Because the price of the blended resin is high, gauge control pays for itself faster on this line than on a commodity film line. An automatic thickness gauge that maps the transverse profile and feeds the die bolts is therefore a practical investment rather than a luxury.
Machine direction and transverse control
Thickness variation has two directions. Machine direction variation usually comes from output pulsation, a wet feed or an unstable melt pump, and shows up as repeating bands along the roll. Transverse variation comes from the die profile, uneven die heating or a chill roll that is not uniform across its face, and shows up as a consistent thin or thick edge. The corrective action is different in each case, so the operator must read the profile map before adjusting anything. Chasing a transverse fault with the screw speed, or a machine direction fault with the die bolts, will make both worse.
11. Slitting, Winding and Roll Behavior
Slitting a soft, water-sensitive film
The cast web is slit to the widths required by the pod forming line, and the slitting operation must produce a clean edge without tearing or heat sealing the film. Sharp blades, correct overlap and low tension are more important here than on a stiffer packaging film, because a soft plasticized web can stretch at the cut and leave a wavy edge that jams a high speed former. Edge trim is collected separately, and because this resin is expensive the trim is either reclaimed in a controlled way or sold, rather than discarded. A slitter that generates excessive trim directly raises the cost per square meter.
Building a stable roll
The winding section builds a roll that will unwind cleanly, sometimes months later and on a machine in another country. Tapered tension is used so that the outer layers are not wound as tightly as the inner layers, which avoids crushing the core and prevents telescoping. Roll hardness must be even across the width, because a soft edge will cause tracking problems at the pod line and a hard band will imprint the film. The winding tension is set in relation to the film’s elongation, and a change in formulation that makes the film softer must be accompanied by a change in winding settings.
12. Sealing and Converting into Pods
How film becomes a pod
On the pod forming line the film is drawn over a mold, heated and vacuum formed into pockets, filled with detergent, and sealed with a second film layer. The seal is made by heat and pressure, and its window is narrow: too little heat gives a leak, too much heat burns or thins a film that is designed to dissolve. Because the film contains PVA, the sealing temperature and dwell have to be matched to the plasticizer level and the moisture content of the web. A film produced correctly on the extrusion line can still fail if the forming line uses settings developed for a different grade.
Seal strength versus dissolution
The pod must stay sealed through handling and storage yet open quickly in water, and these requirements pull in opposite directions. A stronger seal usually needs more heat or a thicker film, both of which slow dissolution and can leave a resistant fragment at the seam. Formulators address this by choosing a dissolution grade matched to the wash temperature and by keeping the seal area narrow. Producers address it by testing the finished pod, not just the film, because the seam is where failure appears. Wanplas recommends running forming trials with production detergent during film qualification, since the product itself affects how the film behaves at the seal.
13. Quality Control and Dissolution Testing
Tests that define a qualified film
A water-soluble film is qualified by a small set of tests that together define whether it will work on the forming line and in the wash. Thickness and basis weight are checked every roll, tensile strength and elongation are measured in both directions, and the coefficient of friction is measured against a standard sled because it predicts how the roll will run. Gel counts and dispersion are checked on a pressed plaque, and moisture is measured at the hopper and on the film. Each test has a defined acceptance band, and a roll outside the band is isolated rather than blended into a good lot.
Dissolution and residue testing
The defining test is dissolution. A sample is placed in water at the specified temperature with a defined agitation, and the operator records the time to first break, the time to full dispersal and whether any visible fragment remains. Water hardness and temperature must be controlled because both change the result. A second test holds the film at the storage humidity for a period and then repeats the dissolution check, since a film that changes with age has not really passed. Wanplas recommends testing the finished pod as well as the film, because the seam and the product inside can change how quickly the package clears.
Seal and aging performance
Because the pod fails at the seal more often than in the body, the quality plan includes a seal strength test on a formed sample and an accelerated storage check at elevated temperature and humidity. The sample is held for a defined period and then examined for leaks, softening and a change in dissolution time. These checks are slower than the inline measurements, so they are run on a schedule rather than on every roll, but they cannot be omitted from a qualification program. A film that passes every online gauge check and fails after four weeks in a warehouse has not met the customer’s requirement.
14. Process Parameters and the Cost of Drift
The settings that control the film
This film has a narrow operating window, and each setting has a measurable cost when it moves outside it. The table below lists typical values for a PLA PVA water-soluble film on a cast line and the consequence of drift. The figures are planning ranges for a production grade and are set precisely during commissioning with the actual formulation and die.
| Parameter | Typical range | Consequence of drift |
|---|---|---|
| Resin moisture at hopper | Below 0.02 percent | Hydrolysis, gels and brittle film |
| Drying air dew point | Minus 30 to minus 40 degrees C | Rewet resin and unstable melt |
| Melt temperature at die | 170 to 210 degrees C by grade | Degradation above, poor melt below |
| Screw speed | 30 to 80 revolutions per minute | Shear heat and dispersion bands |
| Die gap | 0.3 to 0.8 millimeters | Profile shift and unstable web |
| Chill roll temperature | 15 to 40 degrees C | Blocking when warm, haze when cold |
| Film thickness | 20 to 60 micrometers | Seal failure or slow dissolution |
Protecting the window across a shift
A machine that holds these settings through a long shift produces saleable film, while one that needs constant correction produces a mixture of good and downgraded rolls. Closed loop control on drying, melt pressure and die profile reduces operator burden and makes the product more repeatable. Wanplas recommends recording the key settings with each roll and reviewing them when a quality trend appears, because drift is easier to correct as a trend than as a failed lot. This discipline matters more on a water-soluble film than on a robust commodity web.
15. Output, Energy, Scrap and Line Efficiency
Real output of a water-soluble film line
Catalog capacity for a cast film line is usually given in kilograms per hour at a baseline gauge, and a water-soluble film rarely reaches that figure because drying and cooling constrain the line. A 1,200 to 1,600 millimeter line in this class typically runs at a moderate output, and the area produced per hour depends strongly on film thickness. A change from 35 to 25 micrometers increases the area from a given mass of resin but demands better gauge control and gentler handling. Buyers should calculate output from the target gauge and the real line speed rather than accept a headline number based on a thicker film.
Scrap, reclaim and changeover loss
Scrap arises at start up, at grade changes, from edge trim and from any roll that fails a gauge or dissolution check. Edge trim can be recovered in a controlled way, but reprocessed water-soluble resin has a heat history and cannot always be returned at full value, particularly if the formulation is sensitive. Grade changes between cold water and hot water soluble films require a thorough purge because a small carryover changes the dissolution temperature of the next lot. Wanplas recommends scheduling long campaigns for each grade and keeping the changeover record, since lost time and off specification film during transitions are a significant part of the real cost.
16. Cost per Square Meter, Pod Economics and Payback
Building the cost per square meter
The cost of a finished water-soluble film is dominated by the blended resin, with conversion, scrap and depreciation making up the rest. The table below shows a typical cost structure in US dollars per square meter for a 35 micrometer film produced on a medium line. These figures assume a stable formulation, a controlled reclaim rate and a qualified grade, and they move with resin prices, gauge and annual operating hours.
| Cost element | Basis | US dollars per square meter |
|---|---|---|
| Blended resin and plasticizer | 30 to 40 grams at blended price | 0.09 to 0.14 |
| Edge trim, start up and scrap loss | Partly recovered as controlled reclaim | 0.01 to 0.03 |
| Electricity, drying and chilled water | Dryer and casting utilities | 0.02 to 0.04 |
| Labor, slitting, packing and quality | Operating crew and test program | 0.02 to 0.05 |
| Full cash and absorbed cost | Sum including depreciation | 0.15 to 0.28 |
Investment payback
A complete 1,200 to 1,600 millimeter water-soluble film line, including drying, extrusion, die, casting, thickness control and winding, sits broadly in the range of 0.5 to 1.2 million US dollars, with installation and commissioning adding a further margin. At a contribution of a tenth of a US dollar or more per square meter and a steady annual volume, payback is commonly in the range of three to five years. The price of the resin and the stability of the operation matter more than the headline speed of the line, so a buyer should model payback with realistic scrap and changeover losses rather than with catalog output.
17. Wanplas Equipment Recommendation and Buying Checklist
Which Wanplas equipment fits this application
Wanplas supplies cast film extrusion lines that suit water-soluble and biodegradable film, with the drying, metering, melt filtration and thickness control sections this resin family requires. For a laundry pod film in the 1,000 to 1,600 millimeter width range, Wanplas recommends a single screw extruder with a barrier screw, a desiccant dryer with dew point logging, a continuous screen changer with a melt pump, a coat hanger flat die with lip adjustment, a chill roll casting unit and an automatic thickness gauge. The company’s cast film platforms are built for films from about 0.017 to 0.3 millimeters with widths of 1,600 and 2,200 millimeters and duties from roughly 350 to 900 kilograms per hour on conventional resins; for PVA and PLA the configuration is sized to the narrower processing window and lower output of those blends. Only the equipment platform and its process capability are specified here, without invented model codes.
What to settle before signing
Fix the film formulation, the target gauge, the roll width, the dissolution temperature and the sealing conditions before the line is ordered. Then confirm the dryer capacity and dew point, the feeder accuracy, the screw and die geometry, the screen changer and pump, the casting roll arrangement, the thickness control loops, and the slitting and winding setup. The film, the detergent and the pod tooling have to be qualified as one system, so the forming line and the product supplier should see the film specification before the first commercial run. A buyer who settles these points early avoids the most expensive kind of change, which is the one discovered after the resin and the mold have already been committed.
Acceptance test and spare parts
Require a production run with the actual formulation, then verify moisture at the hopper, melt temperature stability, transverse gauge, gel count, tensile properties, blocking after storage and the full dissolution profile at the specified water temperature and hardness. Include a forming trial with the production detergent and a sealed pod storage check, because that is where the package succeeds or fails. Hold a portion of the machine price until the first commercial lot passes at the pod line. Keep spare screen packs, a spare die lip set, feeder parts, dryer desiccant and a set of chill roll bearings, because any one of these can stop a sensitive film line for days when it wears.
Frequently Asked Questions
How much does a PLA PVA water-soluble film extrusion line cost?
A 1,200 to 1,600 millimeter cast film line with desiccant drying, gravimetric feeding, melt filtration, flat die, chill roll casting, thickness control and winding typically costs 500,000 to 1,200,000 US dollars. Installation, commissioning and the first stock of resin add a further margin, and an inline forming and sealing section raises the total substantially.
What is the difference between PLA and PVA in the film?
PVA is the component that dissolves in water and provides the oxygen barrier, while PLA adds stiffness, clarity and cost control but does not dissolve at wash temperature. The blend is tuned so the film stays strong on the shelf and breaks down fully in the wash, with plasticizers and compatibilizers controlling flexibility and dispersion.
Why is drying so important on this line?
PVA absorbs moisture from the air and PLA hydrolyzes when it is wet at melt temperature. Excess moisture causes gels, bubbles and a brittle film that can fail during forming. Resin is normally dried below 0.02 percent moisture, and the drying air dew point is logged with each lot rather than relying on a fixed drying time.
What thickness is a laundry pod film?
Typical thickness is 20 to 60 micrometers, with cold water grades often around 25 to 45 micrometers. A thin film saves resin and dissolves faster but is harder to form without pinholes, while a thicker film is stronger but may miss a short wash cycle. The gauge is set together with the dose and the sealing conditions.
How is dissolution tested?
A sample is placed in water at the specified temperature and agitation, and the operator records the time to first break, the time to full dispersal and any visible residue. Water hardness is controlled, and the test is repeated after storage because a film whose dissolution changes with age has not passed. The finished pod is tested as well as the film.
Can cast and blown film both make water-soluble pod film?
Yes. Cast film offers tight gauge, clarity and high output because a chill roll sets the web quickly, while blown film uses lower cost tooling and gains strength from biaxial orientation. Most high volume pod film is cast where transverse control and forming consistency matter most, but both routes are used commercially.
What causes seal failure in a laundry pod?
Common causes are a sealing temperature or dwell that does not match the plasticizer level, a gauge that has drifted thin, moisture absorbed during storage, and a detergent formulation that softens the film at the seam. Because the failure appears at the pod line rather than at the film machine, qualification must include forming and storage trials with the real product.
What should an acceptance test cover?
Run the line with the actual formulation and verify hopper moisture, melt stability, transverse gauge, gel count, tensile properties, blocking after storage and the full dissolution profile at the specified water temperature and hardness. Include a forming trial with the production detergent and a sealed pod storage check, and hold part of the price until the first commercial lot passes at the pod line.
Conclusion
A PLA PVA water-soluble film extrusion line makes the pouch that turns a laundry pod into a single, disposable dose. PVA supplies dissolution and barrier, PLA supplies stiffness and cost control, and the extrusion line has to deliver a thin, homogeneous web that survives high speed forming and then clears completely in the wash. That combination makes drying, melt stability and gauge control more critical than on an ordinary packaging film.
The economics are driven by resin and by consistency. A 35 micrometer film carries roughly 0.09 to 0.14 US dollars of blended resin per square meter and a full cost near 0.15 to 0.28 US dollars, while a qualified grade sells for 0.25 to 0.45 US dollars. A line in the range of 0.5 to 1.2 million US dollars typically pays back in three to five years, provided the producer controls moisture and scrap rather than chasing extra speed with a thinner gauge.
Wanplas recommends a cast film platform with desiccant drying, a barrier screw, continuous melt filtration, a flat die with lip control, chill roll casting and automatic thickness measurement. Defined around the resin, the film and the pod forming line as one system, the line produces a water-soluble film that seals, stores and dissolves as the customer expects.