The invention discloses a creep-discoloration glass fiber reinforced polypropylene material and a preparation method thereof. The material is prepared from the following components by weight: 72.4–86.5 parts of polypropylene, 10–20 parts of modified glass fiber, 3–6 parts of compatibilizer, 0.3–0.8 parts of lubricant and 0.2–0.8 parts of antioxidant. The modified glass fiber is glass fiber …

The object of the invention is to provide a formulation with improved pharmacokinetics comprising a compound of formula [I] or a pharmaceutically acceptable salt or hydrate thereof, and a preparation method thereof. The invention relates to a solid dispersion comprising an amorphous compound of formula [I] or a pharmaceutically acceptable salt or hydrate thereof, and …

The invention discloses a method for providing a crosslinked composition, comprising the following steps: (a) providing an ethylene-α-olefin plastomer having a density of 850 kg/m³ to 900 kg/m³ and a melt flow rate (ISO 1133, 2.16 kg, 190℃) of 0.3 to 50 g/10 min; (b) grafting the ethylene-α-olefin plastomer with a silane crosslinking agent such …