Contents
1. What a PP Honeycomb Board Extrusion Machine Is and Who Buys One
The machine and the board it makes
A PP honeycomb board extrusion machine is a continuous line that turns polypropylene into a flat, cellular panel with a solid skin on both faces and a regular network of cells between them. The melt leaves a wide die, passes through a calibration and cooling section where the cell structure is set, and is pulled to length by a haul-off and cut into boards. The resulting panel is stiff in bending but far lighter than a solid sheet of the same thickness, because most of its volume is air. It is used where a structure must carry load without adding mass, which is why the automotive interior is one of its most natural markets.
Three buyer groups and their real requirements
The first buyer is a tier one automotive supplier making door panels, parcel shelves, trunk liners or seat backs, whose priority is consistent thickness and a clean, bondable surface. The second is a converter of interior trim who buys board, thermoforms it and laminates decorative layers, and who cares about cell uniformity because it determines how the sheet draws. The third is a general panel producer serving packaging, construction or logistics who wants a machine flexible enough to run several thicknesses and colors. All three buy the same core technology, but the automotive buyer adds documentation, traceability and tighter tolerance requirements to the specification.
2. Why Automotive Interiors Need Lightweight Honeycomb Board
Mass, fuel and electric range
Every kilogram removed from a vehicle reduces fuel consumption over its life and, in an electric vehicle, adds a small amount of driving range. Interior panels are an attractive target because they are large and numerous: door trims, instrument panel carriers, parcel shelves, trunk floors and seat structures together add up to a meaningful share of the non structural mass. A cellular polypropylene board can replace a thicker solid panel or a heavier composite at a fraction of the weight, and it does so without the corrosion or moisture problems of a metal carrier.
Stiffness where it is actually needed
A flat panel resists bending based on its thickness cubed, which is why moving material away from the neutral axis is so effective. Honeycomb and cellular boards put most of the polymer into two thin skins separated by a light core, giving bending stiffness close to a solid sheet at a much lower weight. That is the physical reason a 10 millimeter cellular board can do the work of a substantially heavier solid piece in a door or trunk application. The design task is to place the board so the load runs along the strong direction and to avoid point loads that crush the cells.
3. Honeycomb Board Versus Foam, Solid Sheet and Sandwich Alternatives
Foamed board and solid sheet
Foamed polypropylene board is lighter than solid sheet and easy to produce, but its cells are random and its skin is relatively soft. A cellular honeycomb structure has a more regular load path, better screw retention in the skins and more predictable bending behavior. Solid sheet is the strongest per unit area but inefficient when weight matters. The choice is rarely about which material is strongest; it is about which one meets the stiffness target at the lowest mass and cost for a specific part.
Comparison of common panel routes
The table shows how the main routes compare for an interior panel application. Values are typical ranges for design discussion, and the final choice depends on the part geometry, the load case and the forming process used downstream.
| Panel route | Relative weight | Bending stiffness | Typical interior use |
|---|---|---|---|
| Cellular PP honeycomb board | Low | High for its mass | Door carrier, parcel shelf, trunk liner |
| Foamed PP board | Low to medium | Medium | Insulation, light trim, packaging |
| Solid PP sheet | High | High | Hard trim, covers, masks |
| Fiber reinforced composite | Medium | Very high | Structural carrier, high load part |
4. Cell Structure, Skin Layers and the Mechanics of Lightweighting
How a cellular cross section is formed
The board has two continuous outer skins and an internal network of vertical walls that separate the cells. In an extrusion line this structure is created by the die and the calibration system together: the melt is split into surface streams and internal rib streams, then drawn through a cooling zone that freezes the geometry before the cells can collapse. Cell size and wall thickness are linked to output speed and melt strength. A line running too fast for its cooling length will produce cells that sag or close, and the board will lose stiffness in exactly the direction the designer relied on.
Skin thickness and bending performance
Bending stiffness is dominated by the two skins, so skin thickness is the first variable a designer adjusts. A board with slightly thicker skins and a lighter core can outperform a heavier board with thin skins, because the material is placed where the bending stress is highest. Skin thickness also controls screw and clip retention, which is how interior panels are actually mounted. Wanplas recommends specifying skin thickness and cell wall thickness separately rather than accepting a single nominal density, since two boards with the same weight can behave very differently in a door panel application.
Density, weight per area and where it pays
Cellular polypropylene board typically lands at a few hundred kilograms per cubic meter, far below solid polypropylene at roughly nine hundred. The useful number for an automotive buyer is weight per square meter at a given thickness, because that is what the vehicle mass budget measures. Reducing density further is not always better: a very light board with thin skins may fail a local load test around a mounting point. The most economical design uses the lowest density that still passes the part level tests, leaving the cell structure intact at the fastener locations.
5. PP Resin, Mineral Filler and Additive Cost
Base resin and filler package
A board compound for an interior panel uses a polypropylene with enough melt strength to hold the cell walls during forming. Homopolymer grades give stiffness, while a controlled amount of copolymer improves impact resistance at low temperature, which matters for door panels in cold markets. Mineral filler, usually talc or fine calcium carbonate, raises flexural modulus and reduces cost. Loading of 15 to 40 percent is common, but high filler levels reduce melt strength and make thin cell walls harder to hold, so the compound is a balance between cost and processability rather than a simple cost reduction exercise.
Additives and what they cost
The additive package includes a stabilizer, an antioxidant, a lubricant or processing aid, a nucleating agent for cell control, a color masterbatch and often a flame retardant for interior applications. Interior parts also need low emissions and low odor, which constrains the choice of additives more than mechanical performance alone. Prices range widely: base polypropylene around 1,000 to 1,600 US dollars per ton, mineral filler around 150 to 400, impact modifiers around 1,800 to 3,200, and flame retardant systems around 3,000 to 8,000, with color and stabilizer packages in between.
Why dispersion matters more than the nominal recipe
A correct recipe on paper does not guarantee a good board. If filler agglomerates remain in the melt, they become weak points in the thin cell walls and show up as local collapse or pinholes in the skin. Loss in weight feeders and a well mixed compound are worth more than a small reduction in resin price, because a rejected batch costs far more than the saving. Wanplas recommends running acceptance with the actual production compound rather than a supplier sample, since the filler distribution in a production lot is what determines whether the cell structure stays uniform over a full shift.
6. Complete Line Architecture and Equipment Price List
The stations from feeder to pallet
The line begins with resin and additive feeding, continues through a single screw extruder for the main melt and, where a co-extruded skin is specified, a second smaller extruder. The die forms the skins and cell walls, the calibration table sets the outside gauge, and a multi section cooling trough freezes the structure. A haul-off pulls the board, a flying cut-off divides it to length, and a discharge table collects the panels. Optional stations include edge trimming, surface brushing or corona treatment, and a laminating head if the customer wants a decorated skin applied in line.
Equipment price list
The figures below are delivered equipment prices in US dollars for a line producing 1,220 millimeter wide board in the 3 to 40 millimeter thickness range. Freight, foundations, installation, training and the first set of spare parts are separate. The wide range on the die and calibration items reflects how much of the product family the buyer wants to cover, since each thickness band and skin configuration needs its own tooling setup.
| Line section | Typical price in US dollars |
|---|---|
| Gravimetric feeding and mixing package | 30,000 to 90,000 |
| Main single screw extruder and drive | 120,000 to 320,000 |
| Co-extruder for surface skins | 60,000 to 180,000 |
| Cellular board die and feedblock | 70,000 to 210,000 |
| Vacuum calibration table | 40,000 to 120,000 |
| Cooling trough and water system | 25,000 to 75,000 |
| Haul-off unit | 25,000 to 70,000 |
| Flying cut-off saw and dust collection | 28,000 to 80,000 |
| Edge trim and surface finishing station | 18,000 to 55,000 |
| In-line laminating head | 45,000 to 140,000 |
| Control system and process recording | 30,000 to 85,000 |
| Spare parts and first wear kit | 15,000 to 40,000 |
What the total means in practice
Adding the midpoint of each item gives roughly 0.68 million US dollars, and a realistic project budget adds 50,000 to 110,000 US dollars for site work, installation, commissioning and training. An automotive supplier will usually add process recording and material traceability, which pushes the upper end of the control system range. A packaging board producer can omit the co-extruder and the laminating head and enter at a substantially lower figure, but should recognize that those stations are difficult to add later without rebuilding the downstream frame.
7. Extruder, Die and Co-Extrusion Head
Sizing the main extruder
The main extruder has to deliver a stable melt at high output without overheating a filled polypropylene compound. Wanplas board lines are built around screws in the 65 and 80 millimeter class, corresponding to a 65/132 and an 80/156 configuration, with designed capacity from 450 to 800 kilograms per hour depending on board thickness. The smaller machine suits thinner board and frequent changeovers; the larger one supports continuous production of thick panels. In sizing the drive, a buyer should use the heaviest board in the product plan, because a machine chosen for a thin packaging board will run at its limit on a thick automotive carrier.
Die design and cell formation
The die is the most specialized part of the line. It splits the melt into two surface layers and a set of internal rib streams, then rejoins them at the exit so the board leaves with its skins and cell walls already formed. Flow balance is critical: if one rib stream runs faster than another, the cells lean or close, and the board loses stiffness along one edge. Die temperature is controlled in several zones, and the lip gap is adjusted across the width to compensate for the thicker flow at the center. The result is judged not by the appearance of the exit but by a cross section cut from a cooled sample.
Co-extruded skins and why they matter
A co-extruder feeding a thinner skin layer gives the board a surface with different properties from its core. The core can carry filler for stiffness and low cost, while the skin uses a cleaner, more impact resistant or better bonding polypropylene. For an automotive interior this is valuable because the decorative layer or adhesive must bond to the skin, not to a filler rich surface. The A/B/A configuration in the Wanplas product range uses two skin streams around one core stream. It adds equipment cost but removes a separate surface treatment step and improves repeatability of the bond.
8. Calibration, Cooling and Cell Formation
Setting the outside gauge
The board leaves the die hot and soft, and a vacuum calibration table pulls it against a cooled plate that fixes the external thickness and flatness. Vacuum is applied in zones so the operator can tune the suction from entry to exit. Too much suction at the entry drags the skin and thins one face; too little leaves the board loose and moving, which shows up as a wavy surface. Since bending stiffness depends on skin thickness, the calibration step is directly responsible for whether the board meets its mechanical target, not just its dimensional tolerance.
Cooling length and cell stability
Polypropylene gives up heat slowly, and the cell walls stay soft longer than the skins. The cooling trough is therefore divided into sections with controlled water temperature, and the board must remain supported until the internal structure is rigid enough to carry its own weight. A line that shortens this section to save floor space will produce a board that looks acceptable at the saw but slowly deforms on the pallet. This is why the 3 to 60 millimeter thickness capability of the larger machine is tied to a longer, more capable cooling system rather than to a larger drive alone.
Flatness, bow and internal stress
Uneven cooling between the top and bottom faces creates internal stress, and the board eventually bows toward the side that cooled faster. That bow is a serious problem for thermoforming, because a sheet that is not flat will not clamp evenly in the frame. Wanplas recommends checking flatness after a dwell period rather than immediately at the line, since some stress is released only after the board has fully equalized. Correcting a bow at the forming stage costs far more than adjusting the cooling zones at the extrusion stage.
9. Haul-Off, Cutting and Board Length
Traction without crushing the cells
The haul-off pulls the board through calibration and cooling at a steady speed. traction must be high enough to overcome the drag of the vacuum table but gentle enough not to compress the cellular core, because a crushed cell near the edge permanently reduces local stiffness. Rubber covered caterpillar tracks are common for thick board, while thinner sheet may use roller sets. Wear on the traction surface changes the effective pull and shows up as a gradual drift in board thickness, so the condition of the pads belongs on the routine maintenance list.
Flying cut-off and length tolerance
Interior panel converters usually need board in standard stock lengths, and the cut must be square so the sheet clamps properly in a thermoformer. A flying saw travels with the board while cutting and returns for the next cycle, using a profile encoder for position rather than assuming that haul-off speed is exact. Dust collection at the saw is important because fine polypropylene dust on the surface interferes with later bonding or lamination. The blade should be sharpened on a cut count basis, since filled compounds wear the edge faster than unfilled ones.
10. Skin Bonding, Laminating and Surface Finishing
Why the surface determines the bond
An interior panel is rarely used bare. It is normally thermoformed and combined with a decorative film, a textile or a soft touch layer, so the board surface has to be bondable. A filler rich skin can be difficult to adhesive bond, which is the main reason for specifying a co-extruded clean skin. Surface preparation may include brushing, corona treatment or a light priming step, chosen to match the decorative system. The wrong preparation is expensive because the failure appears months later as a delaminated trim in the field.
In-line laminating and its limits
An in-line laminating head applies a film to the board while it is still traveling, which removes a separate handling step and keeps the surface clean between extrusion and bonding. The variables are film tension, nip pressure and temperature, and the board must be cool and flat before the nip. In-line laminating is most attractive for high volume boards with a single decorative specification. Plants running many short runs often apply the decorative layer after thermoforming instead, because forming a pre-laminated board can stretch the film unevenly over deep corners.
Forming behavior of cellular board
The board is designed to be thermoformed, and the forming behavior is a property of the whole structure. The skins must soften enough to stretch while the cell walls resist collapse, and the heating must be even across the sheet or one side will draw more than the other. A board with inconsistent cell structure will form unevenly even when the oven settings are correct, which is why cell uniformity is an automotive acceptance criterion rather than a cosmetic detail. Wanplas recommends forming trials with production board early in the qualification, before tooling is committed.
11. Quality Control and Automotive Performance Testing
What is measured on the line
Routine checks cover board thickness, width, flatness, skin thickness, cell structure, weight per square meter and surface appearance. Skin thickness and cell uniformity are measured on a cut cross section, because they cannot be judged from the outside. Weight per square meter is the direct link between the board and the vehicle mass budget, so it is tracked by shift. Surface inspection looks for pinholes, lines and discoloration that would show through a decorative layer, with the inspection light set to the same conditions used for the finished interior part.
Performance tests for interior parts
Automotive applications add a layer of testing beyond ordinary board quality. Flexural stiffness and local indentation resistance are checked because they determine whether a panel feels solid when pressed. Low temperature impact, heat aging and dimensional stability under heat matter because a vehicle interior sees a wide temperature range. Flame behavior, odor and emissions are usually specified by the vehicle manufacturer and must be met by the compound as much as by the board structure. Adhesion of the decorative system is tested after aging, not only on the day of bonding.
Traceability and the cost of a complaint
An interior panel complaint can reach far into the supply chain, so automotive buyers expect lot records that connect a board to its compound batch, extrusion conditions and test results. The line controller can store melt temperature, output, line speed and die settings for each production lot. The practical value is the ability to narrow a problem to a shift or a material batch instead of recalling a full production run. Wanplas recommends defining the record format with the customer before commissioning, because adding traceability after an order is placed is both slow and expensive.
12. Process Parameters and the Cost of Deviation
The parameters that control the structure
Melt temperature controls how well the cell walls hold their shape; too low and the rib streams do not weld, too high and the cells sag. Screw speed and haul-off speed together determine output and board thickness. Calibration vacuum fixes the outer gauge, and cooling water temperature fixes how quickly the internal structure becomes stable. Die lip adjustment across the width is the fine control that keeps one edge from running thinner than the other. A deviation in any of these shows up downstream as a stiffness or flatness problem, often after the board has been stacked.
Parameter table
The table gives representative operating windows for a polypropylene cellular board line. These are starting points for trials rather than settings for a specific compound, and the buyer should refine them during acceptance with the actual resin, filler loading and board thickness.
| Parameter | Typical window | Cost of deviation |
|---|---|---|
| Melt temperature | 190 to 230 degrees Celsius | Sagged cells or poor welding |
| Designed capacity | 450 to 800 kg/h | Oversizing raises capital cost |
| Product width | 1,220 mm | Wrong width wastes forming sheet |
| Product thickness | 3 to 40 or 3 to 60 mm | Out of range fails part design |
| Main screw | 65/132 or 80/156 class | Undersizing limits thick board |
| Calibration vacuum | Set by thickness and skin | Thin skin or wavy face |
| Cooling water temperature | Controlled in several zones | Bow after palletizing |
| Die lip setting | Even across the width | Uneven gauge and stiffness |
| Haul-off speed | Matched to output | Thickness drift and scrap |
| Filler loading | 15 to 40 percent | Low melt strength or high cost |
| Laminating nip pressure | Even across the face | Bubbles and weak bond |
Converting settings into money
A small shift in skin thickness can change the mass per square meter enough to affect the vehicle weight target, while a cell structure that collapses under one edge may force the whole board to be downgraded. These losses do not appear as a line stoppage, so they are easy to underestimate. Wanplas recommends assigning a cost per square meter to each quality deviation during commissioning, so the operator can see that holding a stable cooling zone is worth more than pushing output a few kilograms per hour above the design window.
13. Output, Energy, Material Yield and Line Efficiency
What determines real output
Catalog capacity for a honeycomb board line is given in kilograms per hour for a baseline thickness, which makes different machines look comparable when they are not. Real output depends on the board thickness, the skin configuration, the cooling capacity and the stability of the cell structure at speed. A thin 3 millimeter board may run quickly but produces little mass per hour, while a thick 40 millimeter board may be limited by heat removal long before the screw reaches its rating. Wanplas recommends sizing the line from a weighted mix of the intended boards and then checking the thickest panel against the cooling system.
Energy and material yield
The main extruder drive is the largest electrical load, but the co-extruder, feeding, vacuum, cooling water pumps, haul-off and saw add a substantial share. A line of this class typically draws 150 to 300 kilowatts at full production depending on configuration. Material yield is usually high because the process is continuous and the edge trim can be reground, but a filled polypropylene compound loses some melt strength with each reprocessing pass, so the regrind ratio must be controlled. Clean trim from the same compound can return to the core at a limited percentage; contaminated or heavily worked material should be kept out of the skin.
Efficiency in an automotive supply chain
Line effectiveness is shaped less by peak speed than by changeover frequency and qualification stability. A supplier running one board specification for a long campaign will see high utilization, while a plant changing thickness, color and skin configuration several times per shift will spend a significant share of the day in transition. The cost of transition is not only lost output but the material produced while gauge and cell structure settle. Recipe storage, prepared tooling and disciplined changeover are the practical levers, and they matter more in a multi part automotive program than a small increase in nominal extruder size.
14. Cost per Square Meter, Weight Saving Value and Payback
Building the cost of one square meter
Start with material. A 10 millimeter cellular board with an average density near 500 kilograms per cubic meter uses about 5 kilograms of compound per square meter. At a mixed compound cost around 1,100 to 1,500 US dollars per ton, that is roughly 5.5 to 7.5 US dollars of resin per square meter. Energy, labor, tooling amortization and scrap allowance add about 1.0 to 2.0 US dollars, putting conversion cost near 6.5 to 9.5 US dollars per square meter before the decorative layer. A thinner board or a higher filler loading lowers the figure, but not at the expense of the stiffness target.
What the weight saving is worth
The commercial value of cellular board is not only its production cost. Replacing a heavier solid panel or composite carrier reduces vehicle mass, which has a quantifiable value over the life of a vehicle and a direct effect on electric range. An automotive buyer will therefore pay more per square meter for a board that passes the part tests at a lower weight. That is why the selling price of a qualified interior board is not set by the resin price alone. A supplier that can document weight, stiffness and test results is selling an engineering value, which is a much stronger position than selling kilograms of polypropylene.
Investment and payback
A complete 1,220 millimeter line as described in the equipment table represents roughly 0.68 million US dollars in equipment, or 0.73 to 0.79 million with installation, training and the first spare kit. At a contribution of 2 to 5 US dollars per square meter and steady production of two to four million square meters per year, payback falls in the range of 24 to 42 months. A supplier already buying board from an outside converter will recover the investment faster, because the current margin goes to someone else. The sensitivity is utilization and qualification stability, which is why Wanplas recommends confirming the part program before specifying the largest machine.
15. Dust, Volatiles, Fire and Workshop Controls
Dust and housekeeping
A cellular board line generates trim dust at the edge station and the saw, and filled polypropylene dust accumulates quickly in a production hall. Dust collection should be local at each point, with a filter sized for the actual output rather than for the nominal machine. Accumulated dust is a housekeeping problem and a fire risk, particularly when decorative layers or flame retardant compounds are involved. Wanplas recommends a scheduled cleaning route for the die area, the saw enclosure and the filter, because the places that collect dust are often the ones hardest to reach during a production campaign.
Volatiles, temperature and ventilation
Hot polypropylene and additive packages release small amounts of volatiles, and a flame retardant or recycled content compound can release more. Interior board production does not need a cleanroom, but it does need ventilation that keeps the working area comfortable and prevents odor from transferring onto the board surface. Ventilation at the die and the cooling section is more useful than a general room exchange, because it captures material at the point of release. Operator comfort matters here, since a stable process depends on people making small adjustments consistently through a shift.
Fire protection and process safety
The line combines high temperature surfaces, hot melt, electrical drives and combustible dust, which is a standard but real fire risk in extrusion. Hot oil or water heating systems need regular inspection for leaks, and the die area should be kept clear of accumulated material. A fire detection and suppression plan should cover the extrusion head and the dust collection system, not only the building. Wanplas recommends a documented shutdown procedure for a heated die left idle, because the most expensive incidents often happen during an unplanned stop rather than during normal production.
16. Wanplas Equipment Recommendation and Buying Checklist
Which Wanplas equipment fits this application
Wanplas supplies the board extrusion family that matches this task, with a 1,220 millimeter product width, thickness capability from 3 to 40 millimeters and from 3 to 60 millimeters depending on configuration, and designed capacity from 450 to 800 kilograms per hour. The 80/156 main screw handles continuous thick board production, while the 65/132 configuration suits thinner board and more frequent changeovers. The A/B/A co-extrusion arrangement puts a clean skin on a filled core, which is the recommended route when the board will be bonded to an interior decorative layer. Equipment codes shown on the product page are not used here; the configuration is described by width, thickness, screw class and output.
What to settle before signing
Define the board thickness range, skin configuration, density target, compound formulation and the downstream forming or bonding process before the order is placed. Then confirm the die scope, the calibration tooling, the cooling length, the feeding system and whether a co-extruder and in-line laminating head are needed. A supplier may quote a lower price for a machine built around one board thickness, and that machine will struggle the moment the plant adds a thicker carrier or a second skin. Wanplas recommends specifying the whole product family, because the die and the cooling system are the parts that are expensive to change later.
Acceptance test and spare parts
Require a four hour continuous run with the buyer’s own compound, including a cross section check of skin thickness and cell structure, a flatness measurement after a dwell period, and a weight per square meter record across the width. For automotive work, add forming trials and a bond test with the intended decorative system. Hold 10 percent of the machine price until the first commercial lot passes at the customer’s plant. Include a spare die lip set, calibration plate, saw blade, haul-off pads and a set of heated zone components, because each of these can stop a board line for days when it wears out.
Frequently Asked Questions
How much does a PP honeycomb board extrusion machine cost?
A 1,220 millimeter line for thin to medium board typically costs 480,000 to 800,000 US dollars with feeding, die, calibration, cooling and cutting. A configuration with A/B/A co-extrusion, a laminating head and automotive traceability can reach 950,000 US dollars, with installation and training adding 50,000 to 110,000.
What board thickness can this line produce?
Wanplas board configurations cover 3 to 40 millimeters and 3 to 60 millimeters at a 1,220 millimeter width. The exact range depends on the die and calibration tooling supplied, so the buyer should define the full thickness plan before the order rather than buying for the first product only.
How much lighter is honeycomb board than solid polypropylene sheet?
A cellular board at a few hundred kilograms per cubic meter is roughly half the weight of solid polypropylene at about nine hundred. The exact saving depends on skin thickness and cell design, and the useful value for an automotive buyer is weight per square meter at the required stiffness rather than density alone.
Why use a co-extruded skin on a filled core?
Mineral filler lowers cost and raises stiffness, but a filler rich surface bonds poorly to decorative films and adhesives. A co-extruded skin gives a clean, consistent bonding face while the filled core carries the structural and cost function, removing a separate surface treatment step.
What output can a PP honeycomb board line reach?
Designed capacity ranges from 450 to 800 kilograms per hour across the 65/132 and 80/156 screw configurations. Real output depends on board thickness, filler loading and cooling capacity, so the thickest board in the product plan should be used for drive and cooling sizing.
Can Polypropylene Honeycomb Board Be Thermoformed?
Yes, and that is one of its main interior applications. The skins soften while the cell walls resist collapse, so the sheet can be drawn over a tool. Even heating and a uniform cell structure are essential, since an uneven sheet will draw differently from one side.
What causes cells to collapse or lean?
Melt that is too hot loses the strength needed to hold the cell walls, uneven flow in the die makes one rib stream run faster, and a cooling section that is too short lets the structure sag before it sets. Each of these appears as a stiffness or flatness failure rather than a simple cosmetic defect.
What should an acceptance test cover?
Run four hours with the buyer’s compound, then check skin thickness and cell structure on a cross section, flatness after a dwell period, and weight per square meter across the width. For automotive work, add forming trials and an adhesion test with the intended decorative layer, and hold part of the price until the first lot passes.
Conclusion
A PP honeycomb board extrusion machine turns a filled polypropylene compound into a light, stiff cellular panel by placing most of the polymer in two skins separated by a controlled cell structure. The die and cooling system set that structure, so stiffness, flatness and weight per square meter are decided long before the board reaches the thermoforming station.
The economics are driven by the value of weight saving as much as by the cost of resin. Compound at 1,000 to 1,600 US dollars per ton gives a board near 6.5 to 9.5 US dollars per square meter converted, but a qualified panel that passes stiffness and part tests at a lower mass commands a price that resin cost alone cannot explain. A 0.68 million US dollar line can pay back in 24 to 42 months when it stays qualified and utilized.
Wanplas recommends a 1,220 millimeter configuration with an 80/156 main screw for continuous thick board, A/B/A co-extrusion when the board must bond to an interior skin, and a cooling system sized for the thickest panel in the product family. Defined that way, the line delivers a repeatable lightweight board for door carriers, parcel shelves, trunk liners and other automotive interior panels.