1. What a PE Protective Film Extrusion Line for Stainless Steel Sheet Is and Who Buys One
The machine and the film it produces
A PE protective film extrusion line for stainless steel sheet is a cast film system that turns polyethylene pellets into a thin, lightly adhesive web which is laminated onto a metal surface and peeled off later without leaving residue. The film is not a packaging film and not a stretch film. Its job is to act as a sacrificial skin: it takes the scratches, the handling marks, the welding spatter and the warehouse dust so that the stainless steel underneath arrives at the customer with its original finish intact. The line normally includes pellet feeding, one or two extruders, a melt filtration and metering section, a flat die, a chill roll casting station, thickness measurement, corona or priming treatment, slitting, rewinding and a central control panel.
Three buyer groups and their real requirements
The first buyer is a stainless steel coil center or sheet processor that applies film to cut-to-length sheet before delivery; this buyer cares about roll width, peel consistency and a film that can survive weeks of storage. The second is a manufacturer of kitchen equipment, elevator panels, food machinery or architectural cladding that protects parts through forming, laser cutting and assembly; this buyer cares about conformability on tight bends and clean removal after heat exposure. The third is a protective film converter that produces rolls for sale to many metal plants and therefore needs quick grade changes, tight thickness tolerance and a product that behaves the same on brushed, polished and mirror finishes. Each group buys the same family of equipment but specifies a very different recipe and winding setup.
2. What Stainless Steel Surface Protection Actually Has to Do
Scratch protection through the whole chain
Stainless steel is valued for its surface, and that surface is vulnerable from the moment it leaves the mill. Slitting generates burrs and loose metal fragments, stacking slides one sheet over another, and transport vibration turns any trapped grit into an abrasive particle. A protective film of 40 to 80 microns absorbs this damage because it is softer than the metal and sacrificial. The film must be thick enough that a sharp edge does not cut through to the finish, yet thin enough to stay economical and to conform without bubbling. Plants that protect brushed grade sheet usually select 50 to 70 microns; plants handling mirror finish sheet move to 70 to 100 microns and add a softer tie layer.
Adhesion that survives time but still comes off
The central specification is peel force. A film that peels at less than about 0.5 newtons per 25 millimeters will lift at the corners during handling; a film that peels above about 8 newtons per 25 millimeters may transfer adhesive or pull off a delicate brushed finish when removed. Most stainless steel applications sit between 1.5 and 4.5 newtons per 25 millimeters after 24 hours, with lower values for mirror finishes and higher values for rougher hot rolled surfaces. The difficult part is stability: peel force should not double after 30 days in a warm warehouse, and it should not fall away after exposure to humidity. That stability comes from the tackifier system and from cleanliness of the metal surface at application.
3. Film Constructions: Coextruded, Cast and Blown
ABA coextrusion for demanding finishes
In an ABA structure, the outer layers are clean polyethylene that provide strength, low blocking and a controlled surface, while the middle B layer carries the tackifier and can be formulated for release. The result is a film that adheres predictably yet peels cleanly, because the adhesive layer is buried and cannot migrate freely to the surface. A coextruded protective film normally uses a main extruder for the two skin layers and a smaller secondary extruder for the core, with a three layer feedblock and a coat hanger die. On the 1,600 millimeter class of line the main screw is specified at 100 millimeters with a 35 to 1 length to diameter ratio and the secondary screw at 75 millimeters with the same ratio. The extra extruder adds capital cost but removes most residue complaints on polished sheet.
Cast film versus blown film for this application
Cast film is produced by laying the melt curtain onto a chill roll, and it gives excellent thickness uniformity, high clarity and high output, which is why it dominates stainless steel protection. Blown film is cheaper to buy and gives balanced strength in both directions, but gauge variation across a large bubble is greater and the web is less uniform in peel. For a metal sheet that is several meters long, a variation of two microns along the web can be visible as a change in gloss after lamination. Wanplas therefore recommends cast film for mirror, brushed and architectural grades, and reserves blown film for low value hot rolled sheet where appearance is secondary. A blown line remains a reasonable first machine for a converter serving only local fabrication shops.
4. PE Resins, Tackifiers, Additives and Compound Cost
Choosing the base resin
Linear low density polyethylene is the workhorse because it combines puncture resistance with elongation and runs at a stable melt strength on a cast line. Its typical purchase price is 1,050 to 1,450 US dollars per metric ton. Low density polyethylene adds melt strength and improves lay-flat on the chill roll at 1,150 to 1,600 US dollars per ton, while ethylene vinyl acetate with 12 to 18 percent vinyl acetate raises flexibility and cling at 1,600 to 2,400 US dollars per ton. A high clarity protective film for polished sheet often blends 60 to 75 percent linear low density with 15 to 30 percent low density and a small share of ethylene vinyl acetate. A heavy duty film for hot rolled sheet can use more low density and a higher tackifier loading to reduce cost.
The tackifier system and why it dominates performance
Polyisobutylene and hydrogenated hydrocarbon tack resins are the two common routes. Polyisobutylene gives long lasting tack with low migration and sells around 2,000 to 3,200 US dollars per ton, but it is sticky in pellet form and needs careful dosing and a dedicated feeder. Hydrogenated tackifiers are easier to handle and cost 1,800 to 2,900 US dollars per ton, though some grades lose adhesion faster under ultraviolet light. Loading is usually 3 to 9 percent of the adhesive layer. In a three layer film the adhesive core may be only 20 to 30 percent of total thickness, so the effective tackifier share of the whole film is often just 1 to 3 percent, which is one reason coextrusion can lower total formulation cost while improving release.
Compound cost and the make versus buy decision
A 50 micron film at a density near 0.925 grams per cubic centimeter weighs about 0.046 kilograms per square meter. At a blended resin price of 1,250 US dollars per ton, the polymer contributes roughly 0.058 US dollars per square meter, and the additive package adds 0.004 to 0.009, giving a compound cost near 0.062 to 0.067. Buying precompounded pellets raises the purchase price by 80 to 180 US dollars per ton but removes a mixing line and reduces the chance of a dosing error. Plants running one grade for years usually compound in house; converters changing grades several times a week buy precompound and keep two suppliers qualified. The decision should be made on scrap and changeover time, not on pellet price alone.
5. Complete Line Architecture and Equipment Price List
The twelve sections of a complete line
A protective film line is sold as a chain of matched sections. Pellets are unloaded into silos, conveyed gravimetrically to one or two extruders, melted and pushed through a screen changer and a gear pump, distributed by a feedblock into a flat die, laid onto a temperature controlled casting roll, measured by a scanning gauge, treated on the surface, slit to width and wound into rolls that are labeled and wrapped. A line missing any one of these sections still makes film, but it will not make film that a stainless steel customer accepts. The table below gives a realistic budget for a 1,600 millimeter cast line rated at 350 to 400 kilograms per hour, with prices in US dollars for equipment only and a standard industrial finish.
| Line section | What it controls | Typical price in US dollars |
|---|---|---|
| Silo, conveying and gravimetric feeder | Recipe accuracy and pellet hygiene | 45,000 – 110,000 |
| Main extruder, 100 millimeter screw, 35 to 1 | Plasticizing and output stability | 180,000 – 320,000 |
| Secondary extruder, 75 millimeter screw | Tack layer metering | 90,000 – 180,000 |
| Screen changer and melt gear pump | Gel removal and pressure pulsation | 55,000 – 130,000 |
| Three layer feedblock and coat hanger die | Layer uniformity and gauge profile | 85,000 – 190,000 |
| Casting roll, air knife and vacuum box | Surface finish and web pinning | 95,000 – 210,000 |
| Scanning thickness gauge | Cross direction profile control | 48,000 – 130,000 |
| Corona or primer station | Print and laminate adhesion | 18,000 – 55,000 |
| Edge trim and recycling system | Trim recovery and housekeeping | 25,000 – 70,000 |
| Slitter and center winding station | Roll hardness and stripe quality | 75,000 – 170,000 |
| Chiller, air compressor and water loops | Casting temperature stability | 40,000 – 95,000 |
| Control system and data logging | Recipe storage and traceability | 35,000 – 90,000 |
6. Extrusion, Melt Filtration and the Coat Hanger Die
Screw geometry and output
The main extruder on the 1,600 millimeter class has a 100 millimeter screw with a 35 to 1 length to diameter ratio, which gives enough residence length to melt a polyethylene blend uniformly at 350 to 400 kilograms per hour. The secondary extruder uses a 75 millimeter screw at the same ratio to meter the tack layer. Larger 2,200 millimeter lines use a 180 millimeter screw at 30 to 1 and reach 800 to 900 kilograms per hour. The shorter ratio on the large machine is a tradeoff between plasticizing uniformity and residence time; it works because the output is high and the formulation is simple. Barrel zones are normally set from 165 to 215 degrees Celsius, with the die slightly cooler to control sag.
Why filtration decides surface quality
A protective film is laid onto a polished surface, so any hard particle in the melt becomes a visible bump under the web. A continuous screen changer with 25 to 40 micron media and a melt gear pump downstream holds die inlet pressure within plus or minus 1 bar and cuts pulsation below 1 percent. The pump and drive cost 38,000 to 90,000 US dollars at this output, and the screen packs themselves are a running cost of 8,000 to 25,000 US dollars a year depending on resin cleanliness. A plant that recycles its own edge trim should budget at the upper end, because trim pick-up can carry floor dust into the melt.
Feedblock and die lip control
The three layer feedblock splits the flow into skin, core and skin streams and must keep the interface stable when the machine changes output. A coat hanger manifold distributes melt across the full web so that every point at the lip sees the same pressure and temperature. The lip gap is set between 0.25 and 0.60 millimeters before draw down to the final 17 to 300 micron range, using a flexible lip with heated bolts for fine profile correction. An operator who adjusts profile by changing barrel temperature is solving a cross direction problem with a machine direction tool, and the result is usually a second defect. Wanplas commissions this section with a nine point thickness scan across the web and records the bolt map in the recipe.
7. Casting Roll, Web Formation and Surface Finish
The chill roll sets the appearance of the film
The molten curtain leaves the die and lands on a mirror polished chrome roll typically 500 to 900 millimeters in diameter, held at 15 to 35 degrees Celsius by a circulating water circuit with plus or minus 1 degree stability. The roll surface is transferred to the film, so a roll with polishing marks will print those marks into a product used on mirror finished stainless steel. Wanplas measures face temperature at nine positions during commissioning and repeats the map every six months, because a partially blocked water channel produces a cold band that changes both thickness and gloss. A spare chill roll for a two line plant costs 60,000 to 140,000 US dollars and pays for itself in the first surface reject claim.
Draw down ratio and frozen-in stress
Final gauge is reached by drawing the melt away from the die lip faster than it exits, and the ratio between die gap and final thickness is typically 8 to 1 or higher on a thin protective film. Higher draw down improves clarity and orientation but freezes stress into the web, which shows up later as shrinkage on a hot sheet or as corner lift after application. A film that shrinks more than 1.5 percent after 24 hours at 60 degrees Celsius is likely to fail on outdoor panels. The cure is not to slow the line arbitrarily but to balance melt temperature, chill roll temperature and draw ratio, and to verify the result with a heat shrinkage test on every new recipe.
8. Adhesive Systems, Tack Layers and Clean Removal
Coextruded tack layer versus post coating
There are two industrial routes to an adhesive protective film. In coextrusion, the core layer itself contains the tackifier and is buried between two clean skin layers, so adhesion is built into the film during extrusion. In post coating, a neutral film is produced first and a tacky dispersion is applied and dried in a separate coating station. Coextrusion needs the second extruder and feedblock discussed earlier but avoids solvent handling, drying ovens and the associated ventilation cost. Post coating gives a wider range of adhesive chemistry and easier adjustment, but a coating line adds 250,000 to 600,000 US dollars and needs a solvent recovery or abatement system. For stainless steel protection, Wanplas recommends coextrusion as the default route and post coating only where a customer demands a specific pressure sensitive adhesive chemistry.
How thick the tack layer should be
In a three layer film of 60 microns, the core is usually 15 to 20 microns and the two skins together carry the remaining 40 to 45 microns. Making the core thinner reduces peel force and improves removal but can cause the film to lift during storage; making it thicker raises tack and the risk of residue. The relationship is not linear, because the skin layers also control how much tackifier can migrate to the interface. A practical development program runs three core ratios at 20, 28 and 35 percent and measures peel force after 1 day, 14 days and 60 days of aging at 40 degrees Celsius. The grade is chosen on the aged result, not the fresh result.
Removal from brushed, polished and hot rolled surfaces
Adhesion is a property of the pair, not of the film alone. The same roll can peel at 2 newtons per 25 millimeters on a polished surface and 5 newtons on a hot rolled surface because the rougher metal offers more mechanical contact. A converter selling one film to several steel plants will receive complaints from the plant with the roughest finish first. The correct approach is to classify surfaces into finish groups and keep a separate grade for each, with the peel target written against the group rather than against a generic stainless specification. Wanplas recommends keeping three trial panels, polished, brushed and hot rolled, in every plant so that a new lot is checked against all three before shipment.
9. Thickness Tolerance, Gauge Control and Profile
What tolerance the market expects
Stainless steel protection film is normally specified at plus or minus 8 to 10 percent of nominal gauge across the web and plus or minus 5 percent in the machine direction. For a 50 micron film that means roughly 45 to 55 microns, a narrow band that a cast line can hold with a scanning gauge and an automatic die adjustment. A line without automatic profile control can still produce an average of 50 microns while running 43 at one edge and 57 at the other, and the customer will judge it by the thin edge where protection failed. Thickness also drives cost directly: every micron removed from a 50 micron film saves about 0.0012 US dollars per square meter at 1,250 US dollars per ton.
Scanning gauge and closed loop control
A scanning beta or X ray gauge measures basis weight every 10 to 20 millimeters across the web and feeds a profile controller that adjusts the heated die bolts. A single station costs 48,000 to 130,000 US dollars; a two station package with a pre-die measurement reaches 95,000 to 240,000 US dollars. On a 1,600 millimeter protective film line, one station after the casting roll is normally sufficient, with the operator entering the target profile at recipe setup. The gauge should be calibrated with a film sample weighed on a laboratory balance at least once a week, because a drifting sensor will make a good line look bad and can cause unnecessary die adjustments.
The cost of a profile fault
A two micron high band along one edge does not always stop production, but it changes peel force and roll hardness in that band. When the steel plant laminates the film, that band may wrinkle or lift, and the defect appears on the customer’s panel rather than in the converter’s plant. Estimating conservatively, a profile fault that scraps 3 percent of a 400 kilogram per hour shift wastes 12 kilograms per hour, or about 15 US dollars in compound and roughly 60 US dollars in lost finished value. Over 6,000 operating hours that exceeds 300,000 US dollars, several times the price of a gauge system.
10. Winding, Slitting and Roll Quality
Tension taper and roll hardness
A protective film roll that is hard at the core and loose at the outside will telescope in transit; one that is loose at the core will ovalize and feed badly on the customer’s applicator. Center winding with a programmed tension taper reduces tension as the roll diameter grows, keeping internal stress nearly constant. Typical starting tension is 40 to 120 newtons for a 1,000 millimeter web of 50 micron film, tapered by 50 to 70 percent at full roll. The winder, its load cells and the dancer roll add 75,000 to 170,000 US dollars and are worth specifying with spare sensors, because a single failed load cell usually produces a full shift of bad rolls before anyone notices.
11. Application and Lamination Behavior on Metal
How the film behaves on an applicator
On the customer’s sheet line, the film is unwound over a roller train, guided by an edge sensor and pressed onto the metal with a rubber nip. A film with high curl will not track straight, a film with low elongation will wrinkle at the nip, and a film with too much slip will run ahead of the tension control. The extrusion line therefore has to deliver a web that is flat, has balanced stress and carries a consistent release force from the core. Wanplas recommends that converters keep a sample applicator setting sheet for each grade, recording nip pressure, web tension and line speed, and send it with the first shipment to a new customer.
Lamination on curved and formed parts
Flat sheet is the easy case. Fabricated parts such as sink bowls, elevator panels and formed hoods require the film to stretch over a radius without whitening or tearing, and then to stay attached without springing back at the corners. A film with 400 to 600 percent elongation and low heat shrinkage handles most deep draw work, but the adhesive layer must be soft enough to follow the surface. Where forming is severe, applying the film before forming rather than after gives better results and reduces the labor of hand application. The converter should know which route the customer uses before choosing the grade, because the two routes ask for different balances of stiffness and tack.
12. Quality Control and Performance Testing
A test plan that reflects real use
A protective film is judged after weeks of service, not at the moment it leaves the die. A useful test plan therefore combines fast line checks with aging checks that predict field behavior. Line checks include thickness, width, roll hardness and visual gel count; aging checks measure peel force, residue, tensile properties and heat shrinkage after storage at elevated temperature. The table below lists eight tests used on stainless steel protective film, a typical target and an indicative budget for the equipment needed to run them.
| Test | Typical target for stainless sheet | Indicative test setup cost |
|---|---|---|
| 180 degree peel after 24 hours | 1.5 – 4.5 N per 25 mm | 4,000 – 12,000 US dollars |
| Peel after 60 days at 40 degrees C | Less than double the 24 hour value | 3,000 – 8,000 US dollars |
| Residue after removal | No visible transfer on polished panel | 1,000 – 4,000 US dollars |
| Thickness profile scan | Nominal plus or minus 8 percent | Included in line gauge |
| Tensile and elongation at break | 10 – 25 MPa; above 400 percent | 6,000 – 18,000 US dollars |
| Heat shrinkage at 60 degrees C | Below 1.5 percent after 24 hours | 2,000 – 6,000 US dollars |
| Gel and hard particle count | No particle above 40 microns | 8,000 – 25,000 US dollars |
| Abrasion and scratch resistance | No strike-through at specified load | 5,000 – 15,000 US dollars |
Sampling plan and lot records
Every roll should be checked for width, gauge and appearance, while destructive tests are run on the first roll of a lot, every fourth hour of continuous production and the last roll. That schedule catches drift in both directions and keeps laboratory work at a manageable level. A lot record should hold the resin batch, the additive dosing record, the die bolt map, the winding tension curve and the test results, so that a customer complaint can be answered with data. Plants that keep this discipline typically resolve a claim in days; plants that do not often pay for the whole disputed batch.
13. Process Parameters and the Cost of Deviation
The settings that matter most
A cast protective film line has dozens of settings, but twelve determine whether the product is saleable. They fall into four groups: melt preparation, web forming, surface measurement and winding. The table gives a working window for a 50 micron three layer film on a 1,600 millimeter line and a plain language statement of what happens when the value leaves that window. The numbers are starting points for trials rather than universal rules, because resin grade and tackifier chemistry shift the ideal values.
| Parameter | Working window | Cost of deviation |
|---|---|---|
| Barrel temperature | 165 – 215 degrees C | Gels or degraded tackifier and residue risk |
| Melt temperature at die | 205 – 225 degrees C | Sag, gauge swing or poor lay-flat |
| Die inlet pressure | Plus or minus 1 bar | Machine direction gauge bands |
| Screen pack rating | 25 – 40 microns | Hard spots visible on polished sheet |
| Core layer share | 20 – 35 percent | Peel force outside the contract window |
| Die lip gap | 0.25 – 0.60 mm | Edge bead or unstable draw down |
| Chill roll temperature | 15 – 35 degrees C | Gloss difference and curl |
| Water loop stability | Plus or minus 1 degree C | Cross direction thickness band |
| Air knife position | Set by web contact line | Silver streaks and trapped air |
| Draw down ratio | 8 to 1 or higher | Heat shrinkage and corner lift |
| Winding tension | 40 – 120 newtons | Telescoping, oval rolls or blocking |
| Line speed | Matched to 350 – 400 kg/h | Gauge drift and conversion loss |
14. Contamination, Gel Control and Cleanliness
Where contamination enters
Four entry points account for most contamination: recycled trim collected from an unclean floor, pellets opened in a humid warehouse, a screen changer changed late, and a casting roll that has not been cleaned after a color or grade change. Each produces a different defect. Floor dust gives hard black specks, moisture gives bubbles and gels, an overloaded screen gives pressure swings, and a dirty roll gives repeating marks at the roll circumference. Keeping a simple defect photograph log lets an operator identify the entry point within minutes instead of purging the whole line.
15. Output, Energy and Equipment Effectiveness
Output you can actually sell
A 1,600 millimeter line rated at 350 to 400 kilograms per hour does not deliver that figure as saleable film every hour. Allowing for startup waste, grade changes, screen changes and slitter downtime, a realistic overall equipment effectiveness is 65 to 80 percent for a converter with several grades and 80 to 88 percent for a plant running one grade continuously. At 50 microns, 400 kilograms per hour corresponds to about 8,600 square meters of web. Over 3,100 effective hours a year, a single shift plant produces roughly 18 million square meters, while a two shift plant approaches 35 million.
Energy and utility cost
The cast line consumes electricity for extrusion, chill water, air and winding, typically 0.32 to 0.55 kilowatt hours per kilogram of film at this width and output. At 0.10 US dollars per kilowatt hour, that is 35 to 60 US dollars per hour, or 0.0025 to 0.0045 US dollars per square meter for a 50 micron film. Wanplas lines are designed with heat recovery and efficient drives that reduce energy use by around 30 percent compared with a conventional line of the same class, which can save 250,000 to 500,000 US dollars over a ten year life at continuous operation. Chiller maintenance and clean filters are required to keep that advantage.
16. Cost per Square Meter, Selling Price and Payback
Building the unit cost
For a 50 micron three layer film, compound cost is about 0.065 US dollars per square meter, conversion energy 0.0035, labor 0.006 and packaging and freight 0.004, giving a delivered cost near 0.080 US dollars per square meter before scrap and overhead. Adding 4 percent process scrap and plant overhead brings the figure to roughly 0.095 to 0.115. Films sold into mirror finish applications carry a higher formulation cost and a higher price, while heavy gauge film for hot rolled sheet competes closer to 0.10 US dollars per square meter.
Payback on the line
A core investment of 0.90 million US dollars plus installation and working capital brings the project to roughly 1.1 to 1.4 million US dollars. At 18 million salable square meters a year and a contribution of 0.05 US dollars per square meter, the line generates about 0.90 million US dollars a year before fixed overhead, suggesting a payback of 15 to 22 months. Running one grade on two shifts can shorten that to 10 to 14 months; running many short grades with frequent purges can extend it beyond three years. The order book, not the machine, decides the payback.
17. Wanplas Equipment Recommendation and Buying Checklist
Which Wanplas line fits the product
Wanplas supplies cast film extrusion lines in two practical classes for this application. The 1,600 millimeter line handles PP, PE and EVA from 0.017 to 0.3 millimeters at 350 to 400 kilograms per hour, with a 100 millimeter, 35 to 1 main screw and a 75 millimeter secondary screw for the tack layer. The 2,200 millimeter line reaches 800 to 900 kilograms per hour with a 180 millimeter, 30 to 1 screw. Both are suitable for polyethylene protective film; the first suits a converter with several customers and frequent grade changes, the second suits a dedicated contract supplying wide stainless sheet.
Acceptance test and spare parts
Require a four hour run at contracted rate with the production resin, a nine point thickness scan across the web, peel measurements at the start and end of the run, an aged peel check and a residue check on polished, brushed and hot rolled panels. Hold 10 percent of the machine price until the first commercial lot passes at the buyer’s plant. A spare screen changer seal set, a chill roll water pump, a set of trim blades and a spare load cell should be included in the initial order, because each of those items can stop a line for days when it fails.
Frequently Asked Questions
How much does a PE protective film extrusion line cost?
A complete 1,600 millimeter cast line rated at 350 to 400 kilograms per hour costs 620,000 to 1,750,000 US dollars in equipment, with a typical core budget near 900,000. Installation, training and starter spares add 85,000 to 230,000. A 2,200 millimeter line at 800 to 900 kilograms per hour reaches 1.7 to 3.2 million US dollars.
What film thickness is used for stainless steel sheet?
Most indoor protection uses 40 to 70 microns, with 50 microns the common choice. Mirror finish and long outdoor storage move to 70 to 100 microns. The extrusion lines described here cover 0.017 to 0.3 millimeters, so the whole practical range is within one machine platform.
Should the film be coextruded or post coated?
Coextrusion is preferred for stainless steel because the tack layer is buried between clean skin layers, giving stable peel and less residue. Post coating offers more adhesive chemistry but adds a coating and drying station that can cost 250,000 to 600,000 US dollars more.
Why does the same film peel differently on different steel?
Because adhesion depends on the surface as well as the film. A hot rolled finish has more mechanical contact than a polished one, so peel force can be two or three times higher. Grade should be specified against a finish group, and trial panels of each finish should be kept at the plant.
How long can protective film stay on stainless steel?
An indoor film is normally rated for days to a few weeks, while a stabilized outdoor grade is rated for three to six months. The limit is set by tackifier migration and ultraviolet exposure, not by the film tearing. Removal should be tested at the end of the stated life.
Can edge trim be recycled back into the film?
Yes, if it is collected cleanly and kept below about 10 to 15 percent of the feed. Trim picked up from the floor carries dust that becomes visible gel on polished sheet, and trim from a tackifier rich core should be segregated so the recipe stays balanced.
What causes residue after the film is peeled off?
The usual causes are excessive tackifier loading, migration during warm storage, a core layer that is too thick and contamination trapped at the interface. Checking peel force after 60 days at 40 degrees Celsius predicts this problem far better than checking a fresh roll.
What should an acceptance test include before final payment?
Run four hours at contracted rate, take a nine point thickness scan, measure peel at the start and end, check aged peel and inspect residue on polished, brushed and hot rolled panels. Hold 10 percent of the price until the first commercial lot passes at the buyer’s plant.
Conclusion
A PE protective film line for stainless steel sheet is a cast film system judged by adhesion stability and clean removal rather than by output alone. The melt filtration, die profile, chill roll condition and winding taper decide whether the film protects a polished panel through storage and fabrication, and those sections deserve the investment before any optional equipment is added.
The economics favor a coextruded three layer film for most stainless applications. Compound cost near 0.065 US dollars per square meter and delivered cost near 0.10 leave room for a selling price of 0.16 to 0.28, but the margin survives only when aged peel force and residue stay inside the agreed window. A failed film is expensive because the steel panel, not the film, carries the loss.
Wanplas recommends a 1,600 millimeter cast line at 350 to 400 kilograms per hour for a converter serving several metal customers, and a 2,200 millimeter line at 800 to 900 for a dedicated wide sheet contract. Defined with a secondary extruder, scanning gauge and documented acceptance tests, the line can deliver protective film that a stainless steel customer accepts lot after lot.